Not only underpacking but also tensioning of a blanket is of importance. In the case of excessive tensioning, the compressible layer looses its thickness and deforms, which affects the printing properties; in the case of insufficient tensioning, the dot is extended (deformed). Therefore always follow the instructions of machine manufacturers for tensioning values. For a correct and easy blanket tensioning use a torque key.
Under-packing and tensioning:
|
Dimension |
(Nm) |
|
B 3 |
20 - 25 |
|
B 2 |
30 - 35 |
|
B 1 |
40 - 45 |
|
A 0 |
55 -60 |
|
B 0 |
65 - 70 |
|